Anton Paar UNHT³ Standard Ultra Nanoindentation Tester (200 °C)
문의하기
안전한 결제
품질 보장
간편 교환 및 반품
배송 가능
Maximum load [mN]: 50 / 100(1)
Load resolution [nN]: 3
Load noise floor [rms] [μN]: ≤0.05
Loading rate [mN/min]: Up to 1,000
Depth range [μm]: 50 / 100(1)
Depth resolution [nm]: 0.003
Depth noise floor [rms] [nm]: ≤0.03
Data acquisition rate [kHz]: 192
Options
Heating stage up to 200 °C: ✔
Liquid testing: ✔
(1) optional
Measurements under ambient conditions
Variable temperature testing from room temperature up to 200 °C