For full functionality of this site it is necessary to enable JavaScript.
EMIN.VN
0
Product image

SKZ Industrial SKZ1052C 시차 주사 열량계 (0~±500mW)

ModelSKZ1052C
원산지China
문의하기
안전한 결제
품질 보장
간편 교환 및 반품
배송 가능

DSC range: 0~±500mW

Temperature range: -100℃~ 800 ℃ Liquid nitrogen refrigeration

Heating rate: 1 ~ 80 ℃ / min

Cooling rate: 1 ~ 20 ℃ / min (OPTIONAL) (If cooling, For instant cool only, can not be Isothermal below room temperature, and if heating up, can control its rate)

Temperature resolution: 0.1 ℃

Temperature fluctuations:  ±0.1℃

Temperature repeatability: ±0.1℃

DSC noise: 0.01μW

DSC resolution: 0.01μW

DSC accuracy: 0.1 u W

DSC sensitivity: 0.1 u W

Control Mode: Rising temperature, constant temperature(full automatic)

Curve scanning:  Rising scan, cooling scan (OPTIONAL)

Gas flow control: Embedded digital flow meter & Software control, automatic changing

Display: 24 bit 7 inches LCD touch screen display

Data interface: standard USB connector

Parameter standard:  With standard material, with calibration function, the user may correct temperature and heat enthalpy

- Packing List: 

Host instrument 1PC

CD 1PC

Data Line 1PC

Power Line 1PC

Aluminum crucibles 100PCS

Ceramic crucibles 100PCS

Pure tin grains 1bag

Fuse 4A 5PCS

Datasheet