Anton Paar Julia DSC 500 Differential Scanning Calorimeter (ACM)

ModelJulia DSC 500
P/N261470
联系我们
安全结算
品质保证
轻松更换与退货
支持配送

Minimum temperature: ACM: -35 °C; RCM:-90 °C; NCM: -170 °C

Maximum temperature: ACM; RCM: 700 °C; NCM: 600 °C

Maximum heating rate: 300 K/min

Maximum cooling rate: ACM; RCM: 150 K/min; NCM: 200 K/min

Cooling 10 K/min down to: ACM: 5 °C; RCM:-55 °C; NCM: -150 °C

Cooling 5 K/min down to: ACM: -15 °C; RCM:-70 °C; NCM: -160 °C

Temperature accuracy (In): <0.1 K

Enthalpy accuracy (In): <1 %

Measurement range: ± 2,500 mW