Purpose:
Mainly used for determination of stability and performance of the specimens in net perfusion cement slurry, after curing forming and after boiling,.
Technical Parameters:
Max. expansion value with a weight of 300g: ≤17.5±2.5mm
Normal distance between two pointers: 10mm