SKZ Industrial SKZ1052C 差示扫描量热计 (0~±500mW)
DSC range: 0~±500mW
Temperature range: -100℃~ 800 ℃ Liquid nitrogen refrigeration
Heating rate: 1 ~ 80 ℃ / min
Cooling rate: 1 ~ 20 ℃ / min (OPTIONAL) (If cooling, For instant cool only, can not be Isothermal below room temperature, and if heating up, can control its rate)
Temperature resolution: 0.1 ℃
Temperature fluctuations: ±0.1℃
Temperature repeatability: ±0.1℃
DSC noise: 0.01μW
DSC resolution: 0.01μW
DSC accuracy: 0.1 u W
DSC sensitivity: 0.1 u W
Control Mode: Rising temperature, constant temperature(full automatic)
Curve scanning: Rising scan, cooling scan (OPTIONAL)
Gas flow control: Embedded digital flow meter & Software control, automatic changing
Display: 24 bit 7 inches LCD touch screen display
Data interface: standard USB connector
Parameter standard: With standard material, with calibration function, the user may correct temperature and heat enthalpy
- Packing List:
Host instrument 1PC
CD 1PC
Data Line 1PC
Power Line 1PC
Aluminum crucibles 100PCS
Ceramic crucibles 100PCS
Pure tin grains 1bag
Fuse 4A 5PCS
直接联系认证专家