Hangings: 3, 6, or 10 Hangings (3 kinds)
Specimen: See JIS-K7162 or JIS-K6263 for reference
Load Method: Servomotor Type
Weight Load: Max. 5 kN (500 kgf)
Load Detection: Load Cell
Displacement Measurement: Magnetic Linear Scale 1/100 mm,Stroke 0 to Max. ±100 mm
Temperature Range: Max. 200 °C
Software: Windows Compatible
Option: Compression Jig, Bending Jig, Low Temperature Oven, Constant Temperature & Humidity Oven, Divided Oven, Gauge Length Measuring Spec