直接联系认证专家

Temperature Range: Room temperature ~ 600 ℃
Temperature Resolution: 0.001 ℃
Temperature Fluctuation: ±0.01 ℃
Temperature Repeatability: ±0.1 ℃
Heating Rate: 0.1 ~ 100 ℃/min
Cooling Rate: 0.1 ~ 20 ℃/min
Constant Temperature Time: Program setting ≤ 24 h
Curve Scanning: Heating Scan, Cooling Scan
DSC Range: 0 ~ ±800 mW
DSC Resolution: 0.01 μW
DSC Accuracy: 0.001 mW
Temperature Control Modes: Heating, Constant Temperature, Cooling
Power Supply: AC 220 V / 50 Hz (or customizable)
Atmosphere Control Gases: Nitrogen, Oxygen (automatic switching by the instrument)
Gas Flow Rate: 0 ~ 300 mL/min
Gas Pressure: 0.3 MPa
Display: 7-inch LCD touchscreen with 24-bit color
Data Interface: Standard USB port
Parameter Calibration: Supplied with standard reference materials (Indium, Tin, Lead) for user temperature calibration; the instrument features multiple thermocouples, with one set for measuring sample temperature and another for monitoring the internal ambient temperature
Software Features: Includes automatic analysis functionality
Multi-segment Testing: Supports multi-segment heating and cooling programs, with capability for 5-segment program settings