Anton Paar NHT³ Nanoindentation Tester (500mN)

Contact
Secure Checkout
Quality Engagement
Easy change and return
Delivery Available

Maximum load [mN]: 500

Load resolution [nN]: 20

Load noise floor [rms] [μN]: ≤0.5

Loading rate [mN/min]: Up to 10000

Depth range [μm]: 200

Depth resolution [nm]: 0.01

Depth noise floor [rms] [nm]: ≤0.15

Data acquisition rate [kHz]: 192

Options

Liquid testing: ✔