When to test breakdown voltage? Practical experience from lab to factory

2025年11月13日 08時49分15秒

Breakdown voltage represents the limit to which a material can maintain its insulating ability before a discharge occurs. When this value is reduced, the insulation has lost its stability and there is a risk of short circuit, leakage or equipment failure.

Early inspection helps identify the level of aging, manufacturing deviations or environmental influences, especially in parts working in conditions of heat, humidity, or high electrical loads.

The most obvious practical situations when measuring breakdown voltage

- Production: evaluation of input materials, inspection of components after assembly and before shipment.

- Research: determination of dielectric properties of new materials, comparison of results before and after environmental tests.

- Equipment maintenance: inspection of insulation condition of motors, transformers, capacitors, switching devices or old cables.

Common errors and how to fix them

This measurement is prone to error if not performed correctly. Off-center electrode alignment causes uneven field distribution, leading to premature discharge. Poor grounding of the cable or a humid test environment can cause leakage currents on the surface of the sample. Contaminated or greasy samples can also give lower results than the actual results.

The solution lies in controlling the test conditions: keeping the surface dry and clean, adjusting the electrode gap to a stable level, choosing a consistent voltage ramp rate. In addition, the device needs to be periodically calibrated, because errors in the high-voltage measuring circuit can make the entire result invalid.

Read more about breakdown voltage to understand better: If you don't know about breakdown voltage then here is the answer for you.

When to repeat the measurement. Reasonable inspection schedule

Not all materials require frequent testing, but when operating conditions are severe, it is advisable to establish a clear inspection cycle. For production lines, batch testing is common, with each batch representing a shift or batch of material. For equipment operating continuously, re-testing is usually performed after each maintenance period or when abnormalities such as leaks, sparks, or changes in surface temperature are detected.

The results of each measurement should be recorded to monitor the decreasing trend of the breakdown voltage. When the value is found to be decreasing rapidly, it is the basis for assessing the aging level and planning for replacement before a failure occurs. 

Breakdown voltage testing is not a mandatory operation in every process, but is a key step in understanding the insulation condition of electrical materials and equipment. When the measurement data is collected and managed properly, it becomes the basis for maintaining the safety and reliability of the entire electrical system.

関連ニュース

SiC/GaN Semiconductor Material Trends: From Materials Research to In-Depth Failure Analysis
2026年10月24日 09時59分14秒

As we enter the 2026–2030 period, wide-bandgap (WBG) semiconductor materials such as Silicon Carbide (SiC) and Gallium Nitride (GaN) are transforming the power electronics, electric vehicle (EV/HEV), renewable energy, and AI data center industries. The shift from traditional silicon to SiC and GaN enables higher power density, smaller passive components, and improved overall system energy efficiency.

Chauvin Arnoux C.A 6117 Multifunction Electrical Installation Tester
2026年10月23日 15時26分05秒

An all-in-one testing solution that complies with the international standard IEC 60364-6. It features a 5.7-inch color graphical display, supports Type B RCD testing, includes memory for 1,000 measurements, and is equipped with a Lithium-ion battery providing 30 hours of continuous operation

Plastic Products with Color Streaks: How to Adjust Back Pressure and Screw Speed? How Should Color Be Measured to Verify Proper Adjustment?
2026年10月21日 15時30分17秒

In the middle of the night shift, a batch of light-gray plastic emerged, streaked with debris. The machine operator took one look and did what came most naturally: he cranked up the screw speed and increased the back pressure to ensure the orange-colored pellets melted completely. By morning, the color was indeed more uniform. A few weeks later, the customer returned the entire shipment the products had become brittle, cracking at the slightest impact, and the color varied from one delivery to the next, failing to match the approved standard

お得な情報を受け取る

数量割引、まとめ買い価格の更新、新製品情報をメールでお届けします。

登録することで、当社の利用規約およびプライバシーポリシーに同意したものとみなされます。

クイックサポート

認定専門家へ直接アクセス