An analysis of why PP and PE plastics do not hold ink or adhesive, the three mechanisms of plasma surface treatment of plastics, a technical comparison with primer coating, how to verify results quantitatively with a dyne test pen and contact angle measurement, plus genuine surface tension measuring equipment solutions at EMIN Vietnam.
Print a logo on a PP cap, bake it dry, then scratch lightly with a fingernail and the ink peels off in flakes. Stick tape on it and pull it away, and the ink comes off with the tape entirely. Gluing on PE plastic goes the same way: the bond looks solid at first, but a few days later it peels loose on its own. This is a classic challenge for any production engineer who prints or bonds directly onto untreated polyolefin substrates.
Why Are PP and PE So Hard for Ink and Adhesive to Stick To?
Picture the surface of a taro leaf or a PTFE non-stick pan: drop water on it and it immediately beads up instead of spreading. Ink and adhesive on PP and PE plastic behave in exactly the same way. The root cause is that both plastics have a symmetrical, completely non-polar hydrocarbon chain structure, which gives them an extremely low plastic surface energy (only around 30 dyne/cm).

By the surface tension principle, a liquid (ink/adhesive) can spread on its own and bond durably only when the substrate's energy exceeds the liquid's surface tension by at least 7 to 10 mN/m (usually requiring 38 dyne/cm or higher). When surface energy is too low, ink and adhesive only sit loosely on the plastic after drying, with no molecular bond to the substrate. In addition, mold-release additives and a thin organic oil film left from injection molding further reduce adhesion severely.
How Does Plasma Treat a Plastic Surface in 3 Ways at Once?
Plasma is essentially a high-energy activated gas, containing a dense population of ions, free electrons, micro-scale ultraviolet light and highly reactive free radicals. As a plasma stream sweeps over PP and PE plastic, the technology solves the adhesion problem through 3 mechanisms that occur simultaneously:
Active oxygen radicals in the plasma stream collide and react chemically with organic oil films, mold-release agents and dust on the plastic surface, converting them into volatile gases such as CO2 and water vapor, returning a material surface that is pure and clean at the molecular level.
Bombardment by high-energy ions creates micro-cavities at nanometer scale. This structure increases the real contact area many times over, letting ink and adhesive penetrate deeply and form solid mechanical anchor points without dulling, deforming or damaging the appearance of the part's surface.
This is the most critical effect: the plasma stream breaks the inert C-H bonds on the polymer chain and grafts onto them polar functional groups containing oxygen, such as Hydroxyl (-OH), Carbonyl (=O) and Carboxyl (-COOH). These groups act like "chemical magnets", pulling ink and adhesive molecules to spread evenly and forming strong covalent bonds.
Reference: Contact angle / surface tension meters
Technical Comparison: Gas Plasma Technology vs Primer (Chemical Undercoat)
| Criteria | Primer (chemical undercoat) method | Gas plasma treatment solution |
|---|---|---|
| Operating cost | Costly: constant purchases of solvents, wiping rags, fire-safe storage costs. | Maximum savings: the main consumables are electricity and clean compressed air, with periodic maintenance of the emitter head. |
| Speed & line tact | Must be applied by hand and you must wait for the solvent to dry, which bottlenecks the schedule. | Instant treatment (a few milliseconds) right on the automatic conveyor, with no drying wait. |
| Uniformity of the base layer | Depends entirely on the applicator's skill; thick and thin spots easily cause uneven print color. | Precisely 100% repeatable thanks to a robot or conveyor that controls speed and power automatically. |
| Environment & safety | Strong toxic odor, VOC emissions, high fire and explosion risk and health impact on workers. | Green Process: completely chemical-free and friendly to the workshop environment. |
| Risk to the product | An incompatible solvent can yellow, corrode or crack plastic parts. | No material attack: acts only on the top single-molecule layer without changing the plastic's mechanical properties. |
A practical view from EMIN engineers: Note that plasma does not always eliminate 100% of the primer for every special formulation. For plastics with very high internal lubricant content, or especially demanding silicone-based adhesive systems, the best solution may be to combine plasma with an extremely thin primer layer. The most scientific approach is to test directly on the factory's own parts, ink and adhesive before deciding to replace the primer completely.
How Do You Know a Treated Plastic Surface Meets the Adhesion Standard?
This is the quickest tool right on the production floor: use a dyne test pen to draw a test ink line on the spot that just passed under the plasma head. If the ink film stays as a continuous flat line for 2 seconds without beading up, the surface has reached or exceeded the dyne level of that pen (usually chosen in the 38 to 44 dyne/cm range).
A quantitative method for the R&D lab: place a drop of standard liquid (distilled water) on the surface and capture an optical image. Before plasma treatment, the contact angle is large, θ > 90° (hydrophobic surface). After plasma, the water drop flattens and the contact angle drops sharply to θ < 30°, proving that the surface free energy has jumped.
The test that confirms ex-factory quality: actually print ink or apply adhesive on the line and let it dry per the technical standard. Then press test tape (ASTM D3359 standard) onto the print/bond and pull it off quickly at a 90 degree angle. If 100% of the ink or bond remains intact, the process is fully reliable.
The surface activation effect of plasma is not permanent and decays over time (the aging effect, caused by the polymer molecular chains rearranging), lasting from a few hours to a few days depending on the plastic type and ambient temperature. The mandatory technical recommendation is therefore: schedule periodic surface tension checks and install the plasma treatment head right before the printing or glue-dispensing step, and never treat in bulk in advance and then store for several days before printing.
Criteria for Choosing Surface Tension & Contact Angle Measuring Equipment
To accurately evaluate the effectiveness of plastic surface treatment before printing/bonding, equipping the right surface tension measuring equipment is vital for the factory to keep quality uniform and avoid mass peeling defects. QA/QC and R&D engineers should note these 4 core criteria:
The measuring device or test pen set should cover a wide range from 28 to 72 dyne/cm, with high resolution to measure accurately from the native PP/PE substrate to the surface after high-energy activation.
Choose flexibly between a dyne test pen that works in 2 seconds right on the production line, or an automatic optical contact angle meter in the lab for in-depth research.
Prefer pen and test-ink lines certified to DIN ISO 8296 or ASTM D2578, ensuring inspection results are legally valid and repeatable for export shipments.
For an optical contact angle meter, the software should support a high-definition camera, automatic calculation of the angle θ and export of digitized data reports for traceability.
EMIN Vietnam: Specialized Surface Tension & Contact Angle Measurement Solutions
EMIN Vietnam is an authorized distributor of surface tension measuring instruments, automatic optical contact angle meters and dyne test pens to international standards (Arcotest, Tantec...). EMIN's application engineers are ready to help factories test adhesion on your actual PP and PE samples and advise on the best print-quality and bonding control solutions.
View the Surface Tension Measuring Equipment Catalog ➔